ZHANG Fa-ming, CHANG Jiang, BURKEL Eberhard. Dissolution of poly( vinyl alcohol)-modified carbon nanotubes in a buffer solution. New Carbon Mater., 2010, 25(04): 241-243. doi: 10.1016/S1872-5805(09)60030-5
Citation: ZHANG Fa-ming, CHANG Jiang, BURKEL Eberhard. Dissolution of poly( vinyl alcohol)-modified carbon nanotubes in a buffer solution. New Carbon Mater., 2010, 25(04): 241-243. doi: 10.1016/S1872-5805(09)60030-5

Dissolution of poly( vinyl alcohol)-modified carbon nanotubes in a buffer solution

doi: 10.1016/S1872-5805(09)60030-5
More Information
  • Author Bio:

    ZHANG Fa-ming (1978-), male, Dr, Research interests: carbon and related composites, functional porous materials, structure stability and phase transformation,technique and theory of field asssited sintering. Present address: Institute of Physics, University of Rostock, Rostock 18055, Germany. E-mail: star.zhang@163.com, faming.zhang@unirostock.de

  • Corresponding author: CHANG Jiang. Tel: +86-21-52412804; Fax: +86-21-52413903
  • Received Date: 2010-03-17
  • Accepted Date: 2010-08-25
  • Rev Recd Date: 2010-08-03
  • Publish Date: 2010-08-10
  • Multiwalled carbon nanotubes (MWCNTs) were modified with a water-soluble poly( vinyl alcohol) (PVA) polymer (MWCNTs-PVA). The dissolution of the MWCNTs-PVA in Tris-HCl buffer solution was carried out in a shaking water bath by a soaking method. The microstructural changes of the MWCNTs-PVA during soaking was investigated using Fourier transform-infrared spectroscopy, differential scanning calorimetry, transmission electron microscopy, and X-ray diffraction. It is found that part of the MWCNTs-PVA was dissociated into amorphous carbonaceous debris, but most of tubular structures were retained after 21d of soaking. The dissolution process revealed that the C—C bonds of the MWCNTsPVA were broken-down with the generation of carbonaceous debris and residual carbon nanotube layers, and the latter can be further dissociated into amorphous carbonaceous debris. A possible dissolution mechanism of the MWCNTs-PVA in the buffer solution was proposed and discussed. The surface modified MWCNTs have many defects and open C—C bonds on the surfaces of the CNTs. The dissolution of the PVA in the buffer solution leads to a release of carbon atoms on the outer surface of the MWCNTs. It results in a further rupture of the C—C bonds and destroys the tubular structure .
  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Article Metrics

    Article Views(3244) PDF Downloads(1605) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return